New Products
Find Pond Liner, Hdpe Liner, Hdpe Pond Liner on Industry Directory, Reliable Manufacturer/Supplier/Factory from China.
Payment Type: | L/C, T/T, D/P, Western Union, Paypal, Money Gram |
---|---|
Min. Order: | 1000 |
Model No.: geomembrane
Properties | Method | GM 075 | GM 100 | GM 125 | GM 150 | GM 200 | GM 250 | GM 300 | |
Thickness-mil(min.ave) Lowest individual of 10 values | D5199 | 0.75mm | 1.00mm | 1.25mm | 1.50mm | 2.00mm | 2.50mm | 3.00mm | |
(mil)-10% | |||||||||
Density(min)(g/cm³) | D1505 | 0.939 | |||||||
Tensile properties(1)(min.ave) | |||||||||
Yield Strength Breatks Strength Yield Elongation Break Elongation | D6693 | 11KN/m 20KN/m 12% 700% | 15KN/m 27KN/m 12% 700% | 18KN/m 33KN/m 12% 700% | 22KN/m 40KN/m 12% 700% | 29KN/m 53KN/m 12% 700% | 37KN/m 67KN/m 12% 700% | 44KN/m 80KN/m 12% 700% | |
Tear resistance | D1004 | 93N | 152N | 156N | 187N | 249N | 311N | 374N | |
Puncture resistance | D4833 | 240N | 320N | 400N | 480N | 640N | 800N | 960N | |
Stress crack resistance(2) | D5397 | 300hr | 300hr | 300hr | 300hr | 300hr | 300hr | 300hr | |
Carbon black content | D1603 | 2.0-3.% | |||||||
Oxidative Induction Time(OIT)(min.ave.)(5) | |||||||||
(a) Standard OIT or (b) High Pressure OIT | D3895 D5885 | 100 min 400min | |||||||
Oven Aging at 85C (a) Standard OIT(min.ave.)-% retained after 90days or (b) High Pressure OIT(min.ave.)-%retained after 90 days | D3895 D5885 | 55% 80% | 55% 80% | 55% 80% | 55% 80% | 55% 80% | 55% 80% | 55% 80% | |
UV Resistance (a) Standard OIT(min.ave.) or (b) High Pressure OIT(min.ave.)-%retained after 1600hrs(9) | D3895 D5885 | N.R.(8) 50% | N.R.(8) 50% | N.R.(8) 50% | N.R.(8) 50% | N.R.(8) 50% |
Product Categories : Geomembrane